Types of Corrosion 腐蚀类型 1. General (Uniform) Corrosion 1. 全面(均匀)腐蚀 - Metal loss occurs uniformly over the exposed surface - 金属在整个暴露表面均匀地发生损失 - Governed by overall electrochemical kinetics rather than local chemistry - 由整体电化学动力学而非局部化学环境所控制
- 常见于暴露在大气或水环境中的碳钢 - Typically managed by corrosion allowance, coatings, or inhibitors - 通常通过腐蚀余量、涂层或缓蚀剂来控制 2. Pitting Corrosion 2. 点蚀 - Highly localized anodic dissolution at discrete points - 在离散点发生高度局部化的阳极溶解 - Initiated by breakdown of passive films (often due to chlorides or deposits) - 由钝化膜的破裂引发(通常由氯化物或沉积物引起) - Cathodic area is large relative to anodic pit → high local corrosion rate - 阴极区域相对于阳极点蚀坑较大 → 局部腐蚀速率很高 - Major failure mechanism for stainless steels and duplex alloys - 是不锈钢和双相合金的主要失效机制 - Small pits can penetrate full wall thickness rapidly - 小的点蚀坑能快速穿透整个壁厚 3. Microbiologically Influenced Corrosion (MIC) 3. 微生物影响腐蚀 - Corrosion accelerated by microbial metabolic activity - 由微生物代谢活动加速的腐蚀 - Sulphate Reducing Bacteria (SRB) produce sulphides → H₂S generation - 硫酸盐还原菌产生硫化物 → 生成硫化氢 - Creates localized acidic and reducing environments - 造成局部酸性和还原性环境 - Often manifests as deep pitting under biofilms or deposits - 通常表现为生物膜或沉积物下方的深点蚀 4. Galvanic Corrosion 4. 电偶腐蚀 - Occurs when dissimilar metals are electrically connected in an electrolyte - 当不同金属在电解液中电气连接时发生 - Less noble metal becomes anodic and corrodes preferentially - 较不活泼的金属成为阳极并优先腐蚀 - Severity depends on Galvanic series separation, Area ratio (small anode / large cathode = severe attack) - 严重程度取决于电偶序差异、面积比(小阳极 / 大阴极 = 严重腐蚀) - Common failure in bolting, fasteners, mixed-material piping - 常见于螺栓连接、紧固件、混合材料管道中 5. Erosion–Corrosion 5. 冲刷腐蚀 - Combined effect of mechanical wear and electrochemical corrosion - 机械磨损和电化学腐蚀的综合作用 - High-velocity fluids or solids remove protective films - 高速流体或固体去除保护性膜层 - Accelerated metal loss at elbows, tees, valves, chokes - 在弯头、三通、阀门、节流处金属损失加速 - Damage pattern is directional and often horseshoe-shaped - 损坏形态呈定向性,常为马蹄形 6. Crevice Corrosion 6. 缝隙腐蚀 - Localized corrosion in shielded regions with restricted mass transfer - 发生在传质受限的屏蔽区域的局部腐蚀 - Differential oxygen concentration creates anodic crevice interior - 氧浓度差导致缝隙内部成为阳极 - Common under gaskets, flanges, deposits, and lap joints - 常见于垫片、法兰、沉积物及搭接接头下方 - Often more severe than pitting due to stable acidic micro-environment - 由于稳定的酸性微环境,通常比点蚀更严重 7. Stress Corrosion Cracking (SCC) 7. 应力腐蚀开裂 - Synergistic interaction of Tensile stress (applied or residual), Specific corrosive environment and Susceptible material - 拉应力(施加的或残余的)、特定腐蚀环境和敏感材料三者协同作用 - Leads to brittle cracking with little plastic deformation - 导致几乎没有塑性变形的脆性开裂 - Cracks may grow sub-surface and remain undetected - 裂纹可能在表面下扩展且难以探测 8. Hydrogen Induced Cracking (HIC) / Sulphide Stress Cracking (SSC) 8. 氢致开裂 / 硫化物应力开裂 - Associated with hydrogen ingress into steel - 与氢渗入钢中有关 - Common in H₂S-containing environments - 常见于含硫化氢的环境 - Hydrogen accumulates at inclusions → internal cracking - 氢在夹杂物处聚集 → 导致内部开裂 - SSC requires tensile stress; HIC can occur without applied stress - 硫化物应力开裂需要拉应力;氢致开裂可在无外加应力时发生 - Major concern for carbon steel in sour service - 是碳钢在酸性服役环境中的主要关注点 9. Fatigue Corrosion 9. 腐蚀疲劳 - Corrosion-assisted crack initiation and propagation under cyclic loading - 在循环载荷下,腐蚀促进裂纹萌生和扩展 - Common in vibrating piping, rotating equipment, offshore structures - 常见于振动的管道、旋转设备、海上结构 - Surface corrosion pits often act as crack initiation sites - 表面腐蚀点蚀坑常作为裂纹萌生点 10. Corrosion Under Insulation (CUI) 10. 保温层下腐蚀 - External corrosion caused by trapped moisture beneath insulation - 由保温层下积聚的湿气引起的外部腐蚀 - Affects both carbon steel and corrosion-resistant alloys - 影响碳钢和耐腐蚀合金 - Most severe in temperature ranges enabling wet/dry cycling - 在能使干湿交替发生的温度范围内最为严重
|
| 【刷新页面】【打印此文】 【关闭窗口】 |
| 上一篇:表面处理之喷砂,喷丸及抛丸的区别及介绍 下一篇:海工装备重防腐涂料的特点、要求及解决方案! |